MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SMAC SMACFOAM® 1250S-01 Damping Material
Categories: Other Engineering Material

Material Notes: SMAC has developed sound absorbing material dedicated to be used in aerospace and defense activities thanks to its good acoustic properties, its lightweight and its fire resistance properties.

Uses: SMAC is able to propose some expertise in the association of foams and solid materials to optimize insulation properties (mass spring mass system). SMACFOAM® can be used to reduce sound transmission and provide sound absorption in tiny, confined but also wide spaces in aircraft, helicopters, battleship, trucks and trains.

Features:

  • Lightness and acoustic attenuation properties
  • Radiant panel flammability: FAR25-856
  • Max operating temperature: 85°C / 185°F
  • Thermal insulation
  • Hydrophobic treatment of the foam
  • Foam wih fire resistance properties and compression set performance
  • SMACFOAM® panels junction can be made with SMACTAPE®M

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2160 microns
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
 
Descriptive Properties
Insertion Loss14 dB112 Hz
 16 dB
 18 dB
 48 dB
 49 dB
 55 dB
Overall size600 x 1000 mm
Weight0.61 kg/sqm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SMAC SMACWRAP® ST Damping Material, 1 mm
SMAC SMACSONIC® Carbon EX Noise and Vibration Damping
SMAC SMACTANE® SP Damping Material
Asahi Kasei Xyron™ VT31Z PPE/PS, Acoustic Damping
SMAC SMACSIL® 1114S- S02 Damping Material

PZSMAC035 / 146151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.