System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Asahi Kasei Xyron™ VT31Z PPE/PS, Acoustic Damping
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Ether/PPO
;
Polystyrene (PS)
;
Polystyrene + Polyphenylene Ether, Unreinforced
Material Notes:
Excellent heat resistance, flame retardance, dimensional stability, and mechanical properties. Applications: Automotive parts, electrical & electronic parts, industrial parts.
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.16
g/cc
1.16
g/cc
ISO 1183
Filler Content
10 %
10 %
Water Absorption
0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
Immersion; ISO 62
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
150X150X2 mm; Asahi Kasei
Mechanical Properties
Metric
English
Comments
Tensile Strength
50.0
MPa
7250
psi
50% RH; ISO 527
Elongation at Break
30 %
30 %
50%RH, nominal strain; ISO 527
Flexural Strength
88.0
MPa
12800
psi
50% RH; ISO 178
Flexural Modulus
2.47
GPa
358
ksi
50% RH; ISO 178
Charpy Impact, Notched
0.700
J/cm²
@Thickness 4.00 mm
3.33
ft-lb/in²
@Thickness 0.157 in
ISO 179
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
50%RH; IEC 60093
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
50% RH; IEC 60093
Thermal Properties
Metric
English
Comments
CTE, linear
60.0
µm/m-°C
@Temperature -30.0 - 65.0 °C
33.3
µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359
Deflection Temperature at 1.8 MPa (264 psi)
96.0
°C
205
°F
ISO 75-1
Flammability, UL94
V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Melt Temperature
250
-
290
°C
482
-
554
°F
Resin Temperature
Mold Temperature
50.0
-
80.0
°C
122
-
176
°F
Drying Temperature
90.0
-
100
°C
@Time 10800 - 14400 sec
194
-
212
°F
@Time 3.00 - 4.00 hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Asahi Kasei Xyron™ A0210 PA/PPE
Asahi Kasei Xyron™ VN30V PPE/PS, Acoustic Damping
Asahi Kasei Xyron™ AG213 PA/PPE
Asahi Kasei Xyron™ AG512 PA/PPE
Asahi Kasei Xyron™ AT610 PA/PPE
PASAHI8235 / 221262
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.