System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Asahi Kasei Xyron™ AT610 PA/PPE
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Polyphenylene Ether/PPO
Material Notes:
Excellent heat resistance, flame retardance, dimensional stability, and mechanical properties. Applications: Automotive parts, electrical & electronic parts, industrial parts.
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.09
g/cc
1.09
g/cc
ISO 1183
Linear Mold Shrinkage
0.014
-
0.020
cm/cm
0.014
-
0.020
in/in
120X80X3mm; Asahi Kasei
Mechanical Properties
Metric
English
Comments
Tensile Strength
66.0
MPa
9570
psi
50% RH; ISO 527
Elongation at Break
35 %
35 %
50%RH; ISO 527
Flexural Strength
99.0
MPa
14400
psi
50% RH; ISO 178
Flexural Modulus
2.30
GPa
334
ksi
50% RH; ISO 178
Charpy Impact, Notched
2.00
J/cm²
@Thickness 4.00 mm
9.52
ft-lb/in²
@Thickness 0.157 in
ISO 179
Electrical Properties
Metric
English
Comments
Volume Resistivity
4.50e+15
ohm-cm
4.50e+15
ohm-cm
50%RH; IEC 60093
Dielectric Constant
3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength
27.0
kV/mm
@Thickness 2.00 mm
686
kV/in
@Thickness 0.0787 in
short time; IEC 60243
Dissipation Factor
0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 60250
0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
IEC 60250
Thermal Properties
Metric
English
Comments
CTE, linear
90.0
µm/m-°C
@Temperature -30.0 - 65.0 °C
50.0
µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359
Deflection Temperature at 1.8 MPa (264 psi)
113
°C
235
°F
ASTM D648
Processing Properties
Metric
English
Comments
Melt Temperature
280
-
300
°C
536
-
572
°F
Resin Temperature
Mold Temperature
60.0
-
120
°C
140
-
248
°F
Drying Temperature
110
-
130
°C
@Time 7200 - 14400 sec
230
-
266
°F
@Time 2.00 - 4.00 hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Asahi Kasei Xyron™ A0210 PA/PPE
Asahi Kasei Xyron™ TO702 PP/PPE
Asahi Kasei Xyron™ L654V PPE/PS, High Stiffness, Low Warp, High Flow Chassis
Asahi Kasei Xyron™ L564V PPE/PS, High Stiffness, Low Warp, High Flow Chassis
Asahi Kasei Xyron™ L543V PPE/PS, High Stiffness, Low Warp, High Flow Chassis
PASAHI8238 / 221265
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.