MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Celstran® PP-GF30-23 AF 3001 Natural PP, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Celstran PP-GF30-23 is a 30% long glass fiber Polypropylene. The -23 can be used in food contact applications since all of the raw materials contained within are FDA compiant. This material imparts excellent impact and modulus properties that exceed that of short glass fiber polypropylene.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 94.0 MPa13600 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.5 %2.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 6.219 GPa902.0 ksi50mm/min; ISO 527-2/1A
Flexural Strength 158 MPa22900 psiISO 178
Flexural Modulus 6.292 GPa912.6 ksiISO 178
Charpy Impact, Notched 1.95 J/cm²9.28 ft-lb/in²ISO 179/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOL HM2300 PP+GF30%
Celanese SO.F.TER Technoprene® A60K6F Glass-Reinforced Polypropylene
Celanese Celstran® PP-GF30-0455 P10/10 PP, 30% Glass Reinforced
Celanese Celstran® PP-GF30-0453 P10/10 PP, 30% Glass Reinforced
Celanese Celstran® PP-GF30-10 PP, 30% Glass Reinforced

PHCQ219 / 178674

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.