MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOL HM2300 PP+GF30%
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Description: Injection Molding, PP+GF30%, Good Weatherability

Application: Electrical, Electronic and Automotive Parts

CAS: 9003-07-0 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.8 MPa
@Thickness 3.20 mm
12400 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 7.0 %
@Thickness 3.20 mm
7.0 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 118 MPa
@Thickness 6.40 mm
17100 psi
@Thickness 0.252 in
30mm/min; ASTM D790
Flexural Modulus 5.49 GPa
@Thickness 6.40 mm
797 ksi
@Thickness 0.252 in
30mm/min; ASTM D790
Izod Impact, Notched >= 0.785 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
>= 1.47 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
@Thickness 3.20 mm
315 °F
@Thickness 0.126 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190 - 210 °C374 - 410 °FInjection Molding
Middle Barrel Temperature 200 - 230 °C392 - 446 °FInjection Molding
Front Barrel Temperature 200 - 230 °C392 - 446 °FInjection Molding
Nozzle Temperature 210 - 230 °C410 - 446 °FInjection Molding
Melt Temperature 200 - 230 °C392 - 446 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Drying Temperature 70.0 - 80.0 °C158 - 176 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF30-03-Black PP, 30% Glass Reinforced
LG Chemical LUPOL GP2300 PP+GF30%
Techmer ES HiFill® PP GF30 LE 30% Glass Filled
Celanese Celstran® PP-GF30-02 AF 3001 PP, 30% Glass Reinforced
Celanese Celstran® PP-GF30-05 Black PP, 30% Glass Reinforced

PLAY480 / 148490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.