MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 - 1.71 g/ccAverage value: 0.539 g/cc Grade Count:21
Water Absorption 0.750 - 1.10 %Average value: 0.960 % Grade Count:5
Thickness 12000 - 38000 micronsAverage value: 21200 microns Grade Count:12
Linear Mold Shrinkage 0.000500 - 0.0200 cm/cmAverage value: 0.00598 cm/cm Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2.30 - 303 MPaAverage value: 40.6 MPa Grade Count:18
Elongation at Break 1.70 - 11.0 %Average value: 4.25 % Grade Count:4
Flexural Yield Strength 15.3 - 432 MPaAverage value: 78.6 MPa Grade Count:18
Flexural Modulus 0.495 - 15.0 GPaAverage value: 2.90 GPa Grade Count:18
Compressive Yield Strength 2.80 - 7.30 MPaAverage value: 4.86 MPa Grade Count:15
Compressive Modulus 0.0492 - 0.214 GPaAverage value: 0.108 GPa Grade Count:15
Shear Modulus 0.0141 - 0.0438 GPaAverage value: 0.0296 GPa Grade Count:12
Shear Strength 2.80 - 4.50 MPaAverage value: 3.45 MPa Grade Count:12
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 - 26.0 µm/m-°CAverage value: 17.8 µm/m-°C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 213 °CAverage value: 173 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for ABS/Polyurethane Alloy

O5021 / 78457

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.