MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxon Hyjet V
Categories: Fluid; Lubricant

Material Notes: Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability means extent of fluid degradation in aircraft systems will be less than Type IV fluids, in-service fluid life will be longer, and aircraft operator maintenance costs will be lower. HyJet V provides excellent high and low temperature flow properties (kinematic viscosities) and rust protection. HyJet V has also demonstrated an improvement over the erosion protection performance afforded by Type IV fluids.

Exxon HyJet V is designed for use in commercial aircraft phosphate ester hydraulic systems. It meets the SAE AS1241 requirements and is included in the Airbus NSA307110 and Boeing BMS 3-11M qualified products list. It is compatible in all proportions with commercial Type IV and Type V phosphate ester aviation hydraulic fluids.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.998 g/cc
@Temperature 25.0 °C
0.998 g/cc
@Temperature 77.0 °F
ASTM D4052
Density 1.003 g/cc
@Temperature 15.6 °C
0.03624 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 320320Index; ASTM D2270
Viscosity Measure 1400 cSt
@Temperature -54.0 °C
1400 cSt
@Temperature -65.2 °F
Kinematic Viscosity; ASTM D445
Kinematic Viscosity at 40°C (104°F) 10.8 cSt10.8 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.6 cSt3.6 cStASTM D445
Evaporation Loss 15 %15 %6 hr @ 71°C
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050mgKOH/g; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Bulk Modulus 1.448 GPa210.0 ksiIsothermal secant at 100°F/3000psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 250 ohm-cm
@Temperature 20.0 °C
250 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 860 µm/m-°C
@Temperature 25.0 - 100 °C
478 µin/in-°F
@Temperature 77.0 - 212 °F
Specific Heat Capacity 1.76 J/g-°C0.420 BTU/lb-°F
Thermal Conductivity 0.138 W/m-K
@Temperature 40.0 °C
0.957 BTU-in/hr-ft²-°F
@Temperature 104 °F
Pour Point <= -62.0 °C<= -79.6 °FASTM D97
Flammability Test 185185Fire Point [°C]
 >= 427>= 427Auto Ignition [°C]
Flash Point 174 °C345 °FASTM D92
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca 0.00070 %0.00070 %
Chlorine, Cl <= 0.00080 %<= 0.00080 %
H2O, Water 0.10 %0.10 %
Potassium, K 0.0038 %0.0038 %
Sodium, Na 0.00050 %0.00050 %
Sulfur, S 0.0050 %0.0050 %
 
Descriptive Properties
Foam Sequence I, ASTM D11360/0
Foam Sequence II, ASTM D8930/0
Foam Sequence III, ASTM D8930/0
Particle Count, NAS 1638 Class5
Sonic Shear Stability, KV change %21@ 40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil Aero HF
ATI Allvac® 6-6-2 Titanium Alloy, Heat Treatment: 718°C (1325°F) Anneal
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
ATI Allvac® 6-2-4-2-Si UNS R54620 modified Titanium Alloy

WEXXON348 / 75773

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.