MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® 6-6-2 Titanium Alloy, Heat Treatment: 718°C (1325°F) Anneal
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Data provided by Allvac.

Applications: Airframes, jet engines, rocket engine cases, nuclear reactor components, ordnance components.

Key Words: UNS R56620; AMS 4918, 4936, 4971, 4978, 4979. MIL-T-9047, -81556, Ti-6Al-6V-2Sn; Ti-662; Ti-6-6-2; Allvac, an Allegheny Teledyne Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.54 g/cc0.164 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 326326Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 354354Estimated from Rockwell C value.
Hardness, Rockwell C 3535
Hardness, Vickers 341341Estimated from Rockwell C value.
Tensile Strength, Ultimate 966 MPa140000 psi
Tensile Strength, Yield 897 MPa130000 psi0.2% Offset
Elongation at Break 15 %15 %
Reduction of Area 35 %35 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 %5.5 %
Carbon, C 0.050 %0.050 %
Copper, Cu 0.50 %0.50 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe 0.50 %0.50 %
Nitrogen, N 0.020 %0.020 %
Oxygen, O 0.20 %0.20 %
Tin, Sn 2.0 %2.0 %
Titanium, Ti 86 %86 %as balance
Vanadium, V 5.5 %5.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Titanium Ti-6Al-6V-2Sn (Ti-6-6-2) Annealed
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)

NALL48 / 14798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.