MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT + ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.

Applications: Housings, consoles, contact carriers, covers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Test 92 cm³/g0.92 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0027 cm/cm0.0027 in/in60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in60x60x2 mm; ISO 294
Melt Flow 24.65 g/10 min
@Load 2.16 kg,
Temperature 275 °C
24.65 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 120 MPa17400 psi50 mm/min; ISO 527-2
Elongation at Yield 2.1 %2.1 %50 mm/min; ISO 527-2
Modulus of Elasticity 9.60 GPa1390 ksiISO 527-2
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 325 V325 VTest solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 187 °C369 °FISO 75-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection-molding
Mold Temperature 60.0 - 100 °C140 - 212 °F
 
Descriptive Properties
ColorNatural and Black
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT + ASA
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4406 G6 30% Glass Filled PBT

PBASG0102 / 131736

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.