MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Iupilon® S-1000 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: High viscosity. Basic grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics. Superior impact strength. Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC. Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.24 %
@Temperature 23.0 °C
Immersion
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
Melt Flow 7.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaISO-527-1,2
Elongation at Break 105 %ISO 527-1,2
Elongation at Yield 5.5 %ISO 527-1,2
Tensile Modulus 2400 MPaISO 527-1,2
Flexural Strength 93.0 MPaISO 178
Flexural Modulus 2300 MPaISO 178
Charpy Impact Unnotched NBISO 179-1,2
Charpy Impact, Notched 84.0 kJ/m²ISO 179-1,2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmIEC 60093
Surface Resistance 6.00e+15 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 100 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.00 mm
IEC 60243-1
 31.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.00060
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 - 400 VUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 66.0 µm/m-°CISO 11359-2
Maximum Service Temperature, Air 120 °C
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 131 °CISO 75-1,2
Minimum Service Temperature, Air -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupilon® S-2000 Polycarbonate
Mitsubishi Iupilon® FPR 3000 Polycarbonate
Mitsubishi Iupilon® GSH-2030R2 Polycarbonate
Overview of materials for Polycarbonate, 10% Glass Filled
Network Polymers Kepital® F40-03

PMITSU9174 / 191847

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.