Medium viscosity. Basic grade. Used in a wide range of industries, including sports equipment, medical equipment, automobiles, optics, machinery, office automation equipment, and electronics. Superior impact strength. Superior transparency. Usability in a wide range of temperatures: -40degC to 120degC. Excellent precision molding properties and dimensional stability. Superior self-extinguishing properties. Excellent weather resistance. Excellent electrical insulation capabilities.Information provided by Mitsubishi Engineering Plastics Corporation. |