Lewatit® MonoPlus M 500 MB is a strongly basic, gelular anion exchange resin with beads of uniform size (monodisperse) base on a styrene-divinylbenzene copolymer. Due to the monodisperse bead size distribution (uniformity coefficient max 1.1) and a special manufacturing process this resin type is tailor-made for mixed bed application in make-up water system. The special crosslink rate leads to a very high regeneration efficiency paired with a reduced rinse water demand. Lewatit MonoPlus M 500 MB is especially applicable for:- mixed bed application in combination with Lewatit MonoPlus S 108 H
Lewatit MonoPlus M 500 MB is adding special features to the resin bed:- a special bead size distribution ensuring a perfect separation of resin components without cross-contamination
- a good utilization of the total capacity
- a low rinse water demand
- homogenous throughput of regenerants, water and solutions; therefore a homogenous working zone
- sharply contrasting colors
Information provided by Lanxess. |