MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess LEWATIT® MonoPlus M 500 MB Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus M 500 MB is a strongly basic, gelular anion exchange resin with beads of uniform size (monodisperse) base on a styrene-divinylbenzene copolymer. Due to the monodisperse bead size distribution (uniformity coefficient max 1.1) and a special manufacturing process this resin type is tailor-made for mixed bed application in make-up water system. The special crosslink rate leads to a very high regeneration efficiency paired with a reduced rinse water demand. Lewatit MonoPlus M 500 MB is especially applicable for:
  • mixed bed application in combination with Lewatit MonoPlus S 108 H
Lewatit MonoPlus M 500 MB is adding special features to the resin bed:
  • a special bead size distribution ensuring a perfect separation of resin components without cross-contamination
  • a good utilization of the total capacity
  • a low rinse water demand
  • homogenous throughput of regenerants, water and solutions; therefore a homogenous working zone
  • sharply contrasting colors

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.690 g/cc0.0249 lb/in³
Density 1.08 g/cc0.0390 lb/in³
Bead Size 0.570 - 0.670 mm0.0224 - 0.0264 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceYellow, translucent
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8778 / 209170

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.