MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

  • Promotes reliable, steady bulk material flow
  • Abrasion-, chemical- and corrosion-resistant
  • Low coefficient of friction
  • No moisture absorption
  • Reduces or eliminates arching, ratholing and erractic flow

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6969ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Tensile Modulus 0.421 GPa61.0 ksiASTM D638
Flexural Strength 22.1 MPa3200 psiASTM D790
Flexural Modulus 0.500 GPa72.5 ksiASTM D790
Compressive Strength 20.7 MPa3000 psi10% Def.; ASTM D695
Compressive Modulus 0.483 GPa70.0 ksiASTM D695
Izod Impact, Notched NBNBASTM D256 Type A
Coefficient of Friction, Dynamic 0.120.12Dry vs. Steel; QTM55007
Sand Slurry 8.08.01018 Steel = 100
Limiting Pressure Velocity 0.140 MPa-m/sec4000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 90.6 kV/mm2300 kV/inShort Term; ASTM D149
Dissipation Factor 0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C
@Temperature -40.0 - 149 °C
110 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.409 W/m-K2.84 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters LimitedLimited
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)

P1SMP11 / 20161

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.