MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nickel Aluminum Bronze, UNS C63200
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot formability. Fabricated by hot forming and welding.

Applications: nuts, bolts, structural pump parts, shafting requiring corrosion resistance.

Available as rod, bar, and forgings.

Key Words: Copper, CDA 632
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.64 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 92 - 97
Tensile Strength, Ultimate 640 - 725 MPaDepending on amount of cold work or heat treatment
Tensile Strength, Yield 330 - 380 MPaDepending on amount of cold work or heat treatment
Elongation at Break 18 %in 50 mm, 18% reduction in area
Modulus of Elasticity 115 GPa
Compressive Strength 760 MPa
Poissons Ratio 0.32
Machinability 30 %Based on 100% machinability for UNS C360000
Forgeability 70 %
Shear Modulus 44.0 GPa
Charpy Impact 13.0 - 16.0 J
@Temperature -29.0 - 20.0 °C
Keyhole
 23.0 - 27.0 J
@Temperature -29.0 - 20.0 °C
V-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000246 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.04
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.439 J/g-°C
Thermal Conductivity 36.0 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1060 °C
Solidus 1040 °C
Liquidus 1060 °C
Annealing Point 1150 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 705 - 880 °C
Hot-Working Temperature 705 - 925 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 8.0 - 9.5 %
Copper, Cu 75.9 - 84.5 %
Iron, Fe 3.0 - 5.0 %
Lead, Pb <= 0.020 %
Manganese, Mn <= 3.5 %
Nickel, Ni 4.0 - 5.5 %
Other, total <= 0.50 %
Silicon, Si <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nickel Aluminum Bronze, UNS C63000, Annealed Rod
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Copper, UNS C62400 (Aluminum Bronze 11%)

MC63200b1 / 11612

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.