MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C62400 (Aluminum Bronze 11%)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent hot formability for fabrication by hot forging and hot bending.

Applications: bushings, gears, cams, wear strips, nuts, drift pins, tie rods.

Available as flat products and rod.

Key Words: CDA 624
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.45 g/cc0.269 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9292
Tensile Strength, Ultimate 655 MPa95000 psi
Tensile Strength, Yield 330 MPa47900 psi
Elongation at Break 14 %14 %in 50 mm, 11% reduction in area
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3180.318
Fatigue Strength 235 MPa
@# of Cycles 1.00e+8
34100 psi
@# of Cycles 1.00e+8
Reverse Bending; Temper Not Reported
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Forgeability 80 %80 %
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 23.0 J
@Temperature -23.0 - 27.0 °C
17.0 ft-lb
@Temperature -9.40 - 80.6 °F
Temper not specified
Charpy Impact 15.0 J
@Temperature -23.0 - 27.0 °C
11.1 ft-lb
@Temperature -9.40 - 80.6 °F
Keyhole
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
0.0000144 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.341.34
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
9.17 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 58.6 W/m-K
@Temperature 20.0 °C
407 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1025 - 1040 °C1877 - 1900 °F
Solidus 1025 °C1877 °F
Liquidus 1040 °C1900 °F
Annealing Point 593 - 649 °C1100 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 700 °C1110 - 1290 °F
Hot-Working Temperature 760 - 925 °C1400 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10 - 11.5 %10 - 11.5 %
Copper, Cu 82.8 - 88 %82.8 - 88 %
Iron, Fe 2.0 - 4.5 %2.0 - 4.5 %
Manganese, Mn <= 0.30 %<= 0.30 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.25 %<= 0.25 %
Tin, Sn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C62300 (Aluminum Bronze 9%)
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
Nickel Aluminum Bronze, UNS C63200
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Nickel Aluminum Bronze, UNS C63000, HR50 Temper

MC62400b1 / 11606

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.