MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm XT® X800SF Acrylic Based Multipolymer Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes:

Information provided by Cyro Industries

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Water Absorption <= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D551
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 18ASTM D785
Tensile Strength, Yield 46.1 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Elongation at Yield 2.5 %ASTM D638
Tensile Modulus 2.30 GPaASTM D638
Flexural Strength 66.9 MPaASTM D790
Flexural Modulus 2.10 GPaASTM D790
Izod Impact, Notched 1.30 ft-lb/in
@Thickness 6.35 mm,
Temperature 0.000 °C
ASTM D256
 1.80 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°F
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 178 °FASTM D648
Vicat Softening Point 92.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.515ASTM D542
Haze 4.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound
Röhm Acrylite® H10 Acrylic molding and extrusion compound
Asahi Kasei DELPET™ SRB100 Acrylic (PMMA), High Impact
Asahi Kasei DELPET™ 720V Acrylic (PMMA), Standard Grade
LG Chemical HF-380 ABS, High Flow, High Impact

PCYRO53 / 29230

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.