MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Grade, Molded

Material Notes: Data provided by CYRO Industries

Uses: molding applications where clarity, gloss, toughness, and resistance to fatty acids are of primary importance.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Viscosity 2.00e+6 cP
@Shear Rate 100 1/s,
Temperature 240 °C
2.00e+6 cP
@Shear Rate 100 1/s,
Temperature 464 °F
Approximate value
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Spiral Flow 74.0 cm29.1 in215°C; 1/4 in half round channel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ASTM D785
Tensile Strength, Ultimate 61.0 MPa8850 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Tensile Modulus 3.40 GPa493 ksiASTM D638
Flexural Yield Strength 90.0 MPa13100 psiASTM D790
Flexural Modulus 2.80 GPa406 ksiASTM D790
Izod Impact, Notched 0.430 J/cm
@Diameter 6.35 mm
0.806 ft-lb/in
@Diameter 0.250 in
bar; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  1.30 J/g-°C
@Temperature 25.0 °C
0.311 BTU/lb-°F
@Temperature 77.0 °F
 1.90 J/g-°C
@Temperature 100 °C
0.454 BTU/lb-°F
@Temperature 212 °F
 2.30 J/g-°C
@Temperature 175 °C
0.550 BTU/lb-°F
@Temperature 347 °F
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648
Vicat Softening Point 94.0 °C201 °FASTM D1525
Oxygen Index 17.2 %17.2 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5151.515ASTM D542
Haze 4.0 %4.0 %ASTM D1003
Transmission, Visible 84 %84 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 249 °C421 - 480 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Acrylite® H10 Acrylic molding and extrusion compound
Röhm XT® X800SF Acrylic Based Multipolymer Compound
Aluminum 5052-O
Röhm Acrylite® L40 Compound Molding and Extrusion
Röhm ACRYLITE® MD™ L40 Acrylic Polymer For Medical Diagnostics

PCYR27 / 29166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.