MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Firelite 1230 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Insulating Aggregate. Hydraulic bond. A good general purpose medium weight concrete for service up to 1230°C/2240°F. It can be cast or gunned. Conforms to classes P and Q; ASTM classification C-401-84.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.15 g/ccdried to 110°C
Grain Size <= 8000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 2.80 MPaCold Crushing Strength, MST
 2.90 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 3.70 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 4.20 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.280 W/m-KASTM C 417
 0.210 W/m-K
@Temperature 200 °C
ASTM C 417
 0.240 W/m-K
@Temperature 400 °C
ASTM C 417
 0.260 W/m-K
@Temperature 600 °C
ASTM C 417
Maximum Service Temperature, Air <= 1230 °C
Shrinkage 0.60 %MST
 0.30 %
@Treatment Temp. 815 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 36.8 %
CaO 20.3 %
Fe2O3 5.8 %
K2O+Na2O 1.5 %Na2O+ K2O
SiO2 33.1 %
TiO2 1.3 %
 
Descriptive Properties
Net Material Required (kg/m³)1100
Water Addition53 % by weight, 30 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics BTU-GUE
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity
Mid-Mountain Materials CERMEX® PR1000-M Premium Grade Thermal Insulation Paper
Anderman Ceramics EREY99 Yttrium Oxide

CMORF6287 / 203071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.