MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Anderman Ceramics EREY99 Yttrium Oxide
Categories: Ceramic; Oxide

Material Notes: Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance metal melting, oxygen sensors, and semiconductor applications. Products are offered in a wide variety of shapes and sizes.

Key Words: Y2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.95 g/cc0.179 lb/in³
Open Porosity <= 2.0 %<= 2.0 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.50 - 13.7 µm/m-°C4.72 - 7.61 µin/in-°F
Thermal Conductivity 0.300 W/m-K
@Temperature 20.0 - 100 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
Maximum Service Temperature, Air 2000 °C3630 °F
 
Component Elements PropertiesMetricEnglishComments
Y2O3 99.9 %99.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyroboard™ S1300 Roller
Anderman Ceramics EM80P Corundum
Unifrax Excelfrax® 1800 Board Microporous Insulation
Sharadaa Ceramics Resin Bonded Slabs
Advanced Ceramics ALC 1082 (C-786) Alumina

CANDER18 / 104653

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.