MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® ST811HS BK038 PA6-HI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Super Toughened, Heat Stabilized, Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccDAM; ISO 1183
Moisture Absorption 2.30 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.0 MPaDAM; ISO 527-1/-2
Elongation at Yield 29 %DAM; ISO 527-1/-2
Tensile Modulus 400 MPa50% RH; ISO 527-1/-2
 900 MPaDAM; ISO 527-1/-2
Flexural Modulus 850 MPaDAM; ISO 178
Poissons Ratio 0.45DAM
 0.4750% RH
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 80.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 218 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 0.000 °C10°C/min; 50% RH; ISO 11357-1/-2
 50.0 °C10°C/min; DAM; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °COptimum, Extrusion
 235 - 250 °CRange, Extrusion
 260 - 280 °CRange, Injection
 270 °COptimum, Injection
Mold Temperature 70.0 °COptimum, Injection
 50.0 - 90.0 °CInjection
Ejection Temperature 190 °CInjection
Drying Temperature 60.0 °CInjection
 60.0 °CExtrusion
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
 4.00 - 6.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6-I,,M1CG1HR,S14-010
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>PA6-HI<ISO 11469
PolymerPA6-I
Processing Hold Pressure Time (s/mm)4Injection
Regional AvailabilityAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA6-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® ST811HS NC010 PA6-HI
Toyobo PELPRENE™ S3002 Polyester TPE, Ultra Heat-resistant
Celanese Zytel® ST7301 BK356 PA6-HI
Celanese Zytel® ST7301 NC010 PA6-HI
Celanese Zytel® ST801AHS NC010 PA66-HI

PDSX5515 / 198155

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.