MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts ChemSet™ CA5 Cyanoacrylate adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: The ChemSet CA5 is a general-purpose low viscosity cyanoacrylate adhesive useful in wicking or penetrating applications and bonding closely fitted parts. Used in Chip Repair Kits the CA5 is considered "thin-set" which is better for slight nicks, gouges and scrapes on countertop surfaces. Ideal adhesive for high speed production lines.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 lb/gal
Viscosity 1.0 - 3.0 cP
@Temperature 25.0 °C
uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85cured
Shear Strength 700 psiVs. PC. Results vary depending conditions. Substrate failure.; ASTM D1002
 900 psiVs. ABS. Results vary depending conditions. Substrate failure.; ASTM D1002
 900 psiVs. Results vary depending conditions. Substrate failure.; ASTM D1002
 1000 - 1300 psiVs. Aluminum. Results vary depending conditions.; ASTM D1002
 1200 - 1500 psiVs. Zinc. Results vary depending conditions. Cured; ASTM D1002
 1700 - 2000 psiVs. Phenolic. Results vary depending conditions. Substrate failure.; ASTM D1002
 2800 - 3300 psiVs. Steel. Results vary depending conditions.; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°Ccured
Thermal Conductivity 0.100 W/m-Kcured
Glass Transition Temp, Tg 120 °Ccured
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
Shelf Life 12.0 Month
 
Descriptive Properties
Chemical CompositionEthyl Cyanoacrylate
Chemical Resistance100% retainage after immersed 1000 hrs @ 22°C, Air reference
 100% retainage after immersed 1000 hrs @ 22°C, Isopropanol
 110% retainage after immersed 1000 hrs @ 22°C, Ethanol
 110% retainage after immersed 1000 hrs @ 40°C, Motor Oil
 55% retainage after immersed 1000 hrs @ 22°C, Water
 55% retainage after immersed 1000 hrs @ 40°C, 95% RH
 85% retainage after immersed 1000 hrs @ 22°C, Unleaded Gasoline
Colorcolorless, uncured
Gap Filling0.002 inches, cured
Handling Time2 to 5 seconds (Buna N Rubber), cured
 3 to 5 seconds (steel), cured
 5 to 10 seconds (Phenolic), cured
Impact Resistance3 to 7 ft*lb/in2. Cured
Temperature Resistance100% strength retention @ -25°C.
 100% strength retention @ 40°C.
 20% strength retention @ 150°C
 59% strength retention @ 99°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hybrid Plastics POSS® EP 1050 Epoxy Adhesive
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Aptek 6109-A/B Epoxy Encapsulant

PCHEMI903 / 232231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.