MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hybrid Plastics POSS® EP 1050 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: EP1050 is a POSS® based, high-temperature epoxy adhesive with outstanding resistance to ozone, plasma, or atomic oxygen environments. Major applications include medical devices, optics, semiconductors and electronics.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³after cure
Viscosity <= 5000 cP<= 5000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Modulus of Elasticity 3.00 - 3.50 GPa435 - 508 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Glass Transition Temp, Tg 100 - 110 °C212 - 230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 min
@Temperature 80.0 °C
0.100 hour
@Temperature 176 °F
Pot Life 180 min180 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Aptek 6109-A/B Epoxy Encapsulant
Chemical Concepts ChemSet™ CA5 Cyanoacrylate adhesive
Overview of materials for Polyimide
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F

PHYBR030 / 78840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.