Product description: TEGO® Surten W 111 is a non-ionic organic surfactant. Application: TEGO® Surten W 111 improves the wetting properties of aqueous dispersions on difficult substrates and may therefore be used in a variety of applications of pressure sensitive adhesives in high dynamic processes. - Formulation and application of polymer dispersions/latices with fillers or pigments, e. g. paper coatings
- Improves the wetting and spreading properties of aqueous media such as full synthetic and semi synthetic Metal Working Fluids (MWF). Additionally it provides excellent dispersing properties on finely ground aluminium swarf
- In a multitude of other industrial applications where negative interaction between substrates and coatings has to be overcome
Benefits: TEGO® Surten W 111 is a very low foaming wet-ting agent for water based systems. It is solvent and silicone-free. Due to the special selection of active ingredients TEGO® Surten W 111 outperforms conventional wetting agents due to the low foaming behavior and its fast surface migration.Information provided by Evonik |