MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® Surten W 111 Surfactant
Categories: Fluid

Material Notes: Product description: TEGO® Surten W 111 is a non-ionic organic surfactant.

Application: TEGO® Surten W 111 improves the wetting properties of aqueous dispersions on difficult substrates and may therefore be used in a variety of applications of pressure sensitive adhesives in high dynamic processes.

  • Formulation and application of polymer dispersions/latices with fillers or pigments, e. g. paper coatings
  • Improves the wetting and spreading properties of aqueous media such as full synthetic and semi synthetic Metal Working Fluids (MWF). Additionally it provides excellent dispersing properties on finely ground aluminium swarf
  • In a multitude of other industrial applications where negative interaction between substrates and coatings has to be overcome
Benefits: TEGO® Surten W 111 is a very low foaming wet-ting agent for water based systems. It is solvent and silicone-free. Due to the special selection of active ingredients TEGO® Surten W 111 outperforms conventional wetting agents due to the low foaming behavior and its fast surface migration.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
 
Descriptive Properties
Appearancecolorless, clear liquid
Content100%Active matter
Hydroxyl Number66-80 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL570 / 196774

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.