MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP310LS Cotton Fabric  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: Description: NP 310LS is composed of a woven cotton fabric and a specially engineered resin system designed to meet GE A50A341-S8, for low shrink canvas materials. The data presented below is a compilation of IL/Norplex's and two independent test labs results. In all cases, the data from the independent labs was used for the critical specification properties.

Thickness Tested: 0.500"

NP310LS has been replaced by NP342LS

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 - 1.40 g/cc
@Thickness 1.57 mm
ASTM D792
Moisture Absorption at Equilibrium 0.68 %
@Thickness 1.57 mm
ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90 - 110
@Thickness 1.57 mm
ASTM D785
Flexural Strength 17500 psi
@Thickness 1.57 mm
CW; ASTM D790
 18500 psi
@Thickness 1.57 mm
LW; ASTM D790
Izod Impact, Unnotched 1.90 ft-lb/in
@Thickness 12.7 mm
CW, Cond E-48/50; ASTM D256
 2.30 ft-lb/in
@Thickness 12.7 mm
LW, Cond E-48/50; ASTM D256
 
Descriptive Properties
Bond Strength2500 lb0.5", ASTM D229
ColorNatural, Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Garlock 3205 Neoprene/Polyester Fabric
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets
Solvay A85PS Polyester Fabric
Solvay BR100 Nylon fabric
Garlock 3206 Neoprene/Polyester Fabric

PNORPN524 / 48109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.