MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Applied Nanotech Cu-iJ70P Copper Ink
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: ANI’s copper pastes can be used to create high conductivity patterns for applications in the printed electronics industry. ANI’s Cu-iJ70P paste is printed and thermally sintered to form conductive patterns on substrates such as glass, ceramics, and Kapton®. Cu-iJ70P has a high solid content with the small particle size enabling the printing of thick lines and patterns with rapid low energy curing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 60 %60 %
Particle Size 0.070 µm0.070 µm
Viscosity 30000 - 40000 cP30000 - 40000 cP
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000070 - 0.000060 ohm-cm0.0000070 - 0.000060 ohm-cm
 
Descriptive Properties
Conductive Filler TypeCopper (Cu)
Material TypeReady-To-Use Formulation
Recommended Substratesglass, ceramics, and Kapton®
Solvent SystemOrganic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Europrene Latice® 2430 Styrene - Butadiene Copolymer
Versalis Europrene Latice® 5570 Styrene - Butadiene Copolymer
Versalis Europrene Latice® 5577 Styrene - Butadiene Copolymer
Versalis Intex® 131 Styrene - Butadiene Copolymer
Versalis Intex® 132 Styrene - Butadiene Copolymer

PFLEXCM67 / 179469

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.