MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oceanchem Group Tris (chloroethyl) Phosphate (TCEP)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C6H12O4Cl3P

Cas No.: 29716-44-7

Property: It is colorless or light yellow oily transparent liquid with slight cream odor. Soluble in common organic solvents, insoluble in aliphatic hydrocarbon, almost insoluble in water, good hydrolytic stability, slightly decomposed in alkaline solution, no obvious corrosiveness.

Use: It has good performance for fire retarding and plasticity. It can be used as fire retardant for PVC, soft or hard foam polyurethane, cellulose acetate, ethyl cellulose paint, flame-resisting rubber and rubber conveyer belt. Besides self-extinguishing character, it can improve other performances of product, such as water proof, element resistance, antistatic performance, soft feeling, dosage is 5-10 portion, Ol. is 26. It can also be used as special pressure additives for lube, gasoline additives and heat cooling agent of magnesium.

Storage and Packing: In galvanized metal pail. Storage temperature 5-38°C, not over 35°, in dry air. Common chemicals.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 - 1.44 g/cc
@Temperature 204 °C
Viscosity 38 - 47 cP
@Temperature 20.0 °C
Molecular Weight 285.38 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 351 °C
Decomposition Temperature 240 - 280 °C
Flash Point 265.6 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.47 - 1.479n20D
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 37.3 %
Phosphorus, P 10.8 %
 
Descriptive Properties
Acidity<0.20mg KOH/g
AppearanceColorless or light yellow oily transparent liquid
CAS Number29716-44-7
Chroma<100Pt-Co
Molecular FormulaC6H12O4Cl3P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 6969 Duct Tape
Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry
Seals Eastern 7345 Highly Saturated Nitrile Rubber
Mid-Mountain Materials ARMATEX® SF32 Silicone Rubber Coated Glass Fabric
Mid-Mountain Materials ARMATEX® SF10 Silicone Rubber Coated Glass Fabric

POCEAN07 / 104211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.