MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 10B Enriched Boron
Categories: Ceramic

Material Notes: Ceradyne, Inc., a 3M company, uses a unique proprietary process to produce crystalline elemental boron enriched in either 10B or 11B. Because the material only contains boron, maximum utilization of isotope properties is possible. Crystalline 10B, with its high thermal neutron absorption cross section, high isotopic enrichment and lack of other elements in its composition, allows the material to perform at a higher level of thermal neutron absorption performance of any of the possible boron compounds. The high purity of 10B also imparts excellent gamma discrimination. These characteristics make it well suited to neutron detection technologies. In addition, the material has the highest shielding performance of any other available product from Ceradyne, and is useful in applications where limited absorber loading is necessary.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.17 g/cc
Molecular Weight 10.02 g/mol@ 99%
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 10.01294
 
Descriptive Properties
Impurities<10 ppmFe
 <10 ppmCa
 <10 ppmNa
 <10 ppmTa
 <10 ppmTi
 <400 ppmSi
 <5 ppmAl
 1 ppmCu
 2 ppmCr
 2 ppmNi
 4 ppmMg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 1
Titanium, high purity
Titanium Grade 3
Titanium Grade 2
3M 10B Enriched Boron Carbide

PMM40032 / 194923

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.