MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silicon Red Brass, UNS C69400, O60 Temper 13 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Good to excellent corrosion resistance. Excellent hot formability for fabrication by forging, screw machine operations.

Applications: valve stems where corrosion resistance and high strength are critical.

Test specimen: rod - 13mm diameter.

Key Words: CDA 694
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.19 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85
Tensile Strength, Ultimate 621 MPa
Tensile Strength, Yield 310 MPa
@Strain 0.5 %
Elongation at Break 20 %In 50 mm
Modulus of Elasticity 110 GPa
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Forgeability 80 %UNS C37700 (forging brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000280 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 26.0 W/m-K
Melting Point 820 - 920 °C
Solidus 820 °C
Liquidus 920 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 650 °C
Hot-Working Temperature 650 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 80 - 83 %
Iron, Fe <= 0.20 %
Lead, Pb <= 0.30 %
Silicon, Si 3.5 - 4.5 %
Zinc, Zn 14.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Antimonial Naval brass, UNS C46600, H01 (10%) Temper 6 mm rod/bar
Arsenical Naval brass, UNS C46500, H01 (10%) Temper 6 mm rod/bar
Medium leaded naval brass, UNS C48200, O60 Temper 25 mm rod
Phosphorized Admiralty Copper, UNS C44400, Cold Drawn and Annealed
Phosphorized Naval brass, UNS C46700, H01 (10%) Temper 6 mm rod/bar

MC69400b2 / 11702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.