MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Flexible 90401 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Automotive OEM approval(s).

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7515 sec; ASTM D2240
Tensile Strength at Break 14.2 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 310 %Type IV, 510 mm/min; ASTM D638
Tear Strength 36.0 kN/mDie C, 510 mm/min; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Flame Spread 0.00 mm/minAutomotive Burn Test; FMVSS 302
 
Optical PropertiesOriginal ValueComments
Gloss 4.0 %60°; ASTM D523
 
Descriptive Properties
Automotive SpecificationsGM GMP.PVC.077
Cold FlexibilityPassGM 9503P; -29°C, 1.91 mm; 25 mm, 4 hr
FeaturesLow Gloss
Fogging86%SAE J1756; 3 hrs, 212°F(100°C), 70°F(21°C), after 1 hour
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodBlow Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Automotive Interior Trim
Xenon WeatherometerPassSAE J1960; Interior, 1240 kJ/m², All Colors, dE*<3.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness
Geon® Performance Solutions Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible
Fainplast Compounds PMS 96 Flexible PVC, Extrusion
Fainplast Compounds PK 85/N Flexible PVC, Lead Free

PH0POL0273 / 144842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.