MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Wire & Cable W9400 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 373715 sec; ASTM D2240
Tensile Strength, Yield 17.9 MPa2600 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 340 %340 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL Temperature Rating
Brittleness Temperature -18.9 °C-2.02 °FASTM D746
Flammability, UL94  V-2
@Thickness 0.749 mm
V-2
@Thickness 0.0295 in
ALL; UL 94
 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
BK; UL 94
 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
GY; UL 94
 V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
YL; UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
NC; UL 94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
ALL; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 188 °C360 - 370 °F
 
Descriptive Properties
AdditiveLead Stabilizer
Agency RatingsUL QMFZ2
FeaturesFlame Retardant
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable W3400 Polyvinyl Chloride, Flexible
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Axiall 22880 Coax & Telecom Flexible PVC
Geon® Performance Solutions Vinyl Flexible 90401 Polyvinyl Chloride, Flexible
Fainplast Compounds PMS 96 Flexible PVC, Extrusion

PH0POL0224 / 144793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.