MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Sillimanite Powder & Crystal (Al2SiO5)
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Description: Sillimanite is mineral composed of Aluminum and silicon pentoxide. It was named after the chemist B. Silliman (1779-1824). Sillimanite occurs throughout the world in metamorphosed peri-aluminous sedimentary rocks. Used in the manufacture of refractories and high temperature crucibles. Some varieties used in jewelry.
Forms Available: Industrial grade powder and high purity crystals

Information provided by Reade Advanced Materials.

Key Words: Al2SiO5, Fibrolite, Aluminum Silicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.20 g/cc3.20 g/cc
Density 3.241 g/cc0.1171 lb/in³
Molecular Weight 162.04 g/mol162.04 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.0 - 7.06.0 - 7.020°C
 
Thermal PropertiesMetricEnglishComments
Melting Point 1810 °C3290 °F
 
Descriptive Properties
Crystal Structureorthorhombic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EM60P Sillimanite
Aluminum Silicate, Al2SiO5
A. Schulman Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced
Titanium Dioxide, Brookite
Spartech PP5930 Glass/Mica Reinforced Homopolymer

CREADE017 / 1951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.