SABIC® PP 48M10 has good flow characteristics, high stiffness and good impact strength. It is typically used for articles with complex shapes, such as crates and boxes, rigid packaging and components for the automotive and electro-technical industries. This grade is also available with an antistatic additive package, namely SABIC® PP 48M40.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.
This grade material is UL registered under File E111275. IMDS 80775790Information provided by SABIC |