MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC SABIC® PP 48M10 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP 48M10 has good flow characteristics, high stiffness and good impact strength. It is typically used for articles with complex shapes, such as crates and boxes, rigid packaging and components for the automotive and electro-technical industries. This grade is also available with an antistatic additive package, namely SABIC® PP 48M40. The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. This grade material is UL registered under File E111275. IMDS 80775790

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Yield 26.0 MPa3770 psiSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Yield 5.0 %5.0 %ISO 527-2 1A
Tensile Modulus 1.40 GPa203 ksiSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180/1A
 5.00 kJ/m²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 7.00 kJ/m²
@Temperature 0.000 °C
3.33 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 0.700 J/cm²3.33 ft-lb/in²ISO 179/1eA
 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FFlat wise ( testbar 80*10*4mm); ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FFlat wise ( testbar 80*10*4mm); ISO 75
Vicat Softening Point 79.0 °C174 °Fat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 151 °C304 °Fat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentFalse
Nucleating agentFalse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11154 / 244621

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.