MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0160 - 3.63 g/ccAverage value: 2.52 g/cc Grade Count:1514
Porosity 0.0800 - 0.300 %Average value: 0.193 % Grade Count:3
Particle Size 0.0180 - 90.0 µmAverage value: 34.3 µm Grade Count:10
Thickness 30.0 - 202000 micronsAverage value: 3390 microns Grade Count:34
Cell Length 3.00 - 7.00 mmAverage value: 4.67 mm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 12.0 - 230Average value: 96.5 Grade Count:562
Hardness, Knoop 67.0 - 232Average value: 125 Grade Count:346
Hardness, Rockwell A 35.4 - 60.0Average value: 45.2 Grade Count:218
Hardness, Rockwell B 29.0 - 96.0Average value: 69.3 Grade Count:252
Hardness, Vickers 15.0 - 230Average value: 116 Grade Count:369
Tensile Strength, Ultimate 0.700 - 1600 MPaAverage value: 344 MPa Grade Count:883
Tensile Strength, Yield 1.24 - 730 MPaAverage value: 280 MPa Grade Count:788
Elongation at Break 0.130 - 50.0 %Average value: 9.87 % Grade Count:796
Elongation at Yield 2.50 - 15.0 %Average value: 8.30 % Grade Count:4
Reduction of Area 9.00 - 26.0 %Average value: 17.8 % Grade Count:3
Creep Strength 315 - 538 MPaAverage value: 435 MPa Grade Count:6
Rupture Strength 420 - 552 MPaAverage value: 482 MPa Grade Count:6
Modulus of Elasticity 0.0480 - 342 GPaAverage value: 78.2 GPa Grade Count:758
Flexural Yield Strength 172 - 330 MPaAverage value: 260 MPa Grade Count:8
Compressive Yield Strength 0.0532 - 3400 MPaAverage value: 88.6 MPa Grade Count:210
Compressive Modulus 0.0689 - 121 GPaAverage value: 31.5 GPa Grade Count:180
Notched Tensile Strength 90.0 - 414 MPaAverage value: 275 MPa Grade Count:24
Ultimate Bearing Strength 117 - 1090 MPaAverage value: 701 MPa Grade Count:47
Bearing Yield Strength 41.0 - 1100 MPaAverage value: 593 MPa Grade Count:50
Poissons Ratio 0.230 - 0.360Average value: 0.326 Grade Count:528
Fatigue Strength 20.7 - 517 MPaAverage value: 152 MPa Grade Count:241
Fracture Toughness 10.0 - 185 MPa-m½Average value: 47.3 MPa-m½ Grade Count:61
Machinability 10.0 - 90.0 %Average value: 55.9 % Grade Count:264
Shear Modulus 0.0469 - 139 GPaAverage value: 19.9 GPa Grade Count:639
Shear Strength 0.138 - 420 MPaAverage value: 103 MPa Grade Count:668
Charpy Impact 1.00 - 23.0 JAverage value: 7.91 J Grade Count:23
Charpy Impact, Unnotched 16.3 - 77.0 JAverage value: 55.8 J Grade Count:7
Peel Strength 0.241 - 1.25 kN/mAverage value: 0.524 kN/m Grade Count:28
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000260 - 250000 ohm-cmAverage value: 349 ohm-cm Grade Count:642
Magnetic Susceptibility 6.00e-7 - 8.00e-7Average value: 7.61e-7 Grade Count:18
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.68 - 27.4 µm/m-°CAverage value: 22.7 µm/m-°C Grade Count:689
Specific Heat Capacity 0.690 - 1.01 J/g-°CAverage value: 0.902 J/g-°C Grade Count:549
Thermal Conductivity 1.48 - 255 W/m-KAverage value: 149 W/m-K Grade Count:704
Melting Point 184 - 1410 °CAverage value: 606 °C Grade Count:569
Solidus 184 - 660 °CAverage value: 562 °C Grade Count:567
Liquidus 210 - 903 °CAverage value: 644 °C Grade Count:530
Maximum Service Temperature, Air 60.0 - 649 °CAverage value: 193 °C Grade Count:37
Minimum Service Temperature, Air -80.0 - -18.0 °CAverage value: -43.7 °C Grade Count:32
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.0400 - 0.300Average value: 0.0670 Grade Count:10
Reflection Coefficient, Visible (0-1) 0.860 - 0.960Average value: 0.890 Grade Count:12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 505 - 604 °CAverage value: 562 °C Grade Count:4
Melt Temperature 593 - 816 °CAverage value: 732 °C Grade Count:71
Annealing Temperature 177 - 546 °CAverage value: 377 °C Grade Count:285
Solution Temperature 399 - 566 °CAverage value: 512 °C Grade Count:233
Aging Temperature 22.2 - 346 °CAverage value: 169 °C Grade Count:170
Hot-Working Temperature 260 - 510 °CAverage value: 386 °C Grade Count:95
Casting Temperature 616 - 816 °CAverage value: 720 °C Grade Count:70
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 20.0 - 100 %Average value: 92.1 % Grade Count:1537
Antimony, Sb 0.150 - 0.300 %Average value: 0.200 % Grade Count:4
Barium, Ba 0.0100 - 0.100 %Average value: 0.0650 % Grade Count:4
Beryllium, Be 0.000100 - 6.00 %Average value: 0.193 % Grade Count:90
Bismuth, Bi 0.0100 - 11.0 %Average value: 0.793 % Grade Count:71
Boron, B 0.00100 - 11.0 %Average value: 0.570 % Grade Count:66
Cadmium, Cd 0.00200 - 0.200 %Average value: 0.0321 % Grade Count:6
Calcium, Ca 0.000900 - 22.0 %Average value: 2.02 % Grade Count:15
Carbon, C 0.0300 - 0.350 %Average value: 0.168 % Grade Count:4
Chromium, Cr 0.00300 - 21.0 %Average value: 0.182 % Grade Count:739
Cobalt, Co 0.00100 - 10.0 %Average value: 1.37 % Grade Count:12
Copper, Cu 0.00300 - 52.0 %Average value: 1.50 % Grade Count:1423
Cr + Mn 0.100 - 0.800 %Average value: 0.406 % Grade Count:16
Cr + Mn + Ti + V 0.0250 - 0.0300 %Average value: 0.0258 % Grade Count:6
Gallium, Ga 0.00500 - 0.0500 %Average value: 0.0301 % Grade Count:47
Iron, Fe 0.00600 - 50.0 %Average value: 0.635 % Grade Count:1405
Lead, Pb 0.00300 - 9.00 %Average value: 0.351 % Grade Count:105
Lithium, Li 0.000900 - 4.20 %Average value: 1.53 % Grade Count:51
Magnesium, Mg 0.00500 - 52.0 %Average value: 1.31 % Grade Count:1349
Manganese, Mn 0.00200 - 26.0 %Average value: 0.364 % Grade Count:1318
Nickel, Ni 0.0100 - 50.0 %Average value: 0.886 % Grade Count:280
Oxygen, O 0.0500 - 0.600 %Average value: 0.318 % Grade Count:19
Phosphorus, P 0.00100 - 0.0100 %Average value: 0.00770 % Grade Count:10
Potassium, K 1.00 %Average value: 1.00 % Grade Count:5
Scandium, Sc 0.0100 - 0.800 %Average value: 0.329 % Grade Count:6
Si+Fe 0.0200 - 1.00 %Average value: 0.623 % Grade Count:59
Silicon, Si 0.000 - 80.0 %Average value: 3.14 % Grade Count:1434
Silver, Ag 0.0500 - 30.0 %Average value: 2.95 % Grade Count:40
Sodium, Na 0.000900 - 0.500 %Average value: 0.281 % Grade Count:9
Strontium, Sr 0.00500 - 16.0 %Average value: 2.16 % Grade Count:26
Tin, Sn 0.0200 - 22.0 %Average value: 1.12 % Grade Count:151
Titanium, Ti 0.00200 - 11.0 %Average value: 0.216 % Grade Count:1082
V+Ti 0.00400 - 0.0300 %Average value: 0.0196 % Grade Count:14
Vanadium, V 0.00500 - 11.0 %Average value: 0.277 % Grade Count:139
Zinc, Zn 0.000 - 50.0 %Average value: 1.18 % Grade Count:1327
Zirconium, Zr 0.0100 - 16.0 %Average value: 0.335 % Grade Count:214
Zr+Ti 0.0800 - 0.500 %Average value: 0.207 % Grade Count:30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Aluminum, Al
Overview of materials for Copper Alloy
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 6000 Series Aluminum Alloy

M01039 / 81664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.