MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) SOLVAir® Select 300 Sodium Bicarbonate
Categories: Other Engineering Material

Material Notes:

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.30 g/ccTypical
 1.22 - 1.38 g/cc
Particle Size 214 µmTypical, D50
 96 - 333 µmD50
 258 - 314 µmD90
 436 µmTypical, D90
Particle Mesh Size 67 MeshUS>= 100 (150 µm), Typical
 37 - 97 MeshUS>= 100 (150 µm)
 85 MeshUS>= 200 (75 µm), Typical
 70 - 100 MeshUS>= 200 (75 µm)
 83 - 100 MeshUS>= 325 (45 µm)
 92 MeshUS>= 325 (45 µm), Typical
Molecular Weight 84.01 g/mol
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Content<1.1%H2O Insoluble
 >97%NaHCO3
 0.5%H2O Insoluble, Typical
 99%NaHCO3, Typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY689 / 218417

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.