MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) SOLVAir® Select 300 Sodium Bicarbonate
Categories: Other Engineering Material

Material Notes:

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.30 g/cc0.0470 lb/in³Typical
 1.22 - 1.38 g/cc0.0441 - 0.0499 lb/in³
Particle Size 214 µm214 µmTypical, D50
 96 - 333 µm96 - 333 µmD50
 258 - 314 µm258 - 314 µmD90
 436 µm436 µmTypical, D90
Particle Mesh Size 67 Mesh67 MeshUS>= 100 (150 µm), Typical
 37 - 97 Mesh37 - 97 MeshUS>= 100 (150 µm)
 85 Mesh85 MeshUS>= 200 (75 µm), Typical
 70 - 100 Mesh70 - 100 MeshUS>= 200 (75 µm)
 83 - 100 Mesh83 - 100 MeshUS>= 325 (45 µm)
 92 Mesh92 MeshUS>= 325 (45 µm), Typical
Molecular Weight 84.01 g/mol84.01 g/mol
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Content<1.1%H2O Insoluble
 >97%NaHCO3
 0.5%H2O Insoluble, Typical
 99%NaHCO3, Typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLVAY689 / 218417

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.