Physical Properties | Original Value | Comments |
---|
Density | 0.00545 - 1.95 g/cc |
Filler Content | 0.000 - 40.0 % |
Water Absorption | 0.0400 - 2.00 % |
| 0.260 - 3.15 % @Temperature 50.0 - 80.0 °C |
| 0.300 - 3.29 % @Temperature 50.0 - 80.0 °C |
| 0.300 - 3.29 % @Time 86400 - 173000 sec |
Moisture Absorption at Equilibrium | 0.0200 - 3.90 % |
Water Absorption at Saturation | 0.420 - 4.00 % |
| 2.30 - 4.17 % @Temperature 80.0 - 80.0 °C |
Viscosity | 8.00 - 16.0 cP @Temperature 360 - 360 °C |
| 8.00 - 16.0 cP @Load 5.00 - 5.00 kg |
Thickness | 5.00 - 127 microns |
Linear Mold Shrinkage | 0.000100 - 0.0140 cm/cm |
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0140 cm/cm |
Melt Flow | 2.00 - 37.0 g/10 min |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Rockwell E | 20.0 - 91.0 |
Hardness, Rockwell M | 20.0 - 125 |
Hardness, Rockwell R | 74.0 - 129 |
Hardness, Shore D | 65.0 - 93.0 |
Ball Indentation Hardness | 138 - 345 MPa |
Tensile Strength, Ultimate | 0.0480 - 345 MPa |
| 23.0 - 324.054 MPa @Temperature 150 - 260 °C |
Tensile Strength, Yield | 15.0 - 230 MPa |
| 27.579 - 141.343 MPa @Temperature 149 - 260 °C |
Elongation at Break | 0.350 - 200 % |
| 1.70 - 90.0 % @Temperature 150 - 260 °C |
Elongation at Yield | 2.00 - 90.0 % |
| 4.00 - 90.0 % @Temperature 149 - 149 °C |
Modulus of Elasticity | 0.107 - 46.9 GPa |
| 1.03421 - 3.71627 GPa @Temperature 260 - 260 °C |
Flexural Yield Strength | 24.8 - 490 MPa |
| 20.6843 - 344.738 MPa @Temperature 149 - 260 °C |
Flexural Modulus | 1.38 - 40.0 GPa |
| 0.0102 - 30.3 GPa @Temperature 149 - 300 °C |
Flexural Strain at Break | 1.30 - 5.50 % |
Flexural Strain at Yield | 1.40 - 7.90 % |
Compressive Strain at Break | 12.0 - 54.0 % |
| 21.0 - 31.0 % @Temperature 260 - 260 °C |
Compressive Yield Strength | 0.00217 - 570 MPa |
| 71.0 - 414 MPa @Temperature 149 - 260 °C |
| 96.0 - 172 MPa @Temperature 260 - 260 °C |
| 96.0 - 172 MPa @Strain 10.0 - 10.0 % |
Compressive Modulus | 0.00164 - 7.94 GPa |
| 1.663 - 2.997 GPa @Temperature 260 - 260 °C |
Poissons Ratio | 0.250 - 0.410 |
| 0.320 - 0.320 @Temperature 190 - 190 °C |
Fatigue Strength | 16.5474 - 26.2001 MPa @# of Cycles 1000 - 1.00e+7 |
| 16.5474 - 26.2001 MPa @Temperature 260 - 260 °C |
Shear Strength | 81.4 - 90.0 MPa |
| 78.5 - 78.5 MPa @Temperature 150 - 150 °C |
Izod Impact | 25.0 - 69.0 J |
| 38.0 - 74.0 J @Temperature -30.0 - -30.0 °C |
Izod Impact, Notched | 0.0700 - 9.20 J/cm |
Izod Impact, Unnotched | 0.900 - 5340 J/cm |
Izod Impact, Notched (ISO) | 0.0430 - 27.0 kJ/m² |
| 4.00 - 5.00 kJ/m² @Temperature -30.0 - -30.0 °C |
Izod Impact, Unnotched (ISO) | 0.320 kJ/m² - NB |
| 147 kJ/m² - NB @Temperature -30.0 - -30.0 °C |
Charpy Impact Unnotched | 0.540 J/cm² - NB |
| 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
Charpy Impact, Notched | 0.110 - 1.60 J/cm² |
Dart Drop, Total Energy | 33.0 J |
Coefficient of Friction | 0.0600 - 0.490 |
Coefficient of Friction, Static | 0.200 - 0.350 |
K Factor (Wear Factor) | 0.400 - 13.1 |
Compression Set | 12.5 - 98.0 % |
|
Electrical Properties | Original Value | Comments |
---|
Electrical Resistivity | 0.100 - 4.00e+19 ohm-cm |
Surface Resistance | 0.100 - 1.00e+18 ohm |
Dielectric Constant | 1.11 - 62.0 |
Dielectric Strength | 3.00 - 305 kV/mm |
Dissipation Factor | 0.0000400 - 0.310 |
Dielectric Loss Index | 0.00180 - 0.0106 |
Comparative Tracking Index | 125 - 399 V |
Hot Wire Ignition, HWI | 30.0 - 120 sec |
High Amp Arc Ignition, HAI | 0.000 - 15.0 arcs |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 4.30 - 72.0 µm/m-°C |
| 0.234 - 144 µm/m-°C @Temperature 15.6 - 400 °C |
CTE, linear, Transverse to Flow | 4.70 - 55.0 µm/m-°C |
| 36.0 - 70.0 µm/m-°C @Temperature 50.0 - 300 °C |
Specific Heat Capacity | 0.925 - 1.24 J/g-°C |
| 0.895376 - 1.42256 J/g-°C @Temperature 60.0 - 300 °C |
Thermal Conductivity | 0.0330 - 4.47 W/m-K |
| 0.220 - 2.05 W/m-K @Temperature 40.0 - 300 °C |
Melting Point | 247 - 388 °C |
Maximum Service Temperature, Air | 200 - 395 °C |
Hot Ball Pressure Test | 125 °C |
Deflection Temperature at 0.46 MPa (66 psi) | 215 - 377 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 196 - 470 °C |
Vicat Softening Point | 221 - 260 °C |
Minimum Service Temperature, Air | -240 - -20.0 °C |
Glass Transition Temp, Tg | -20.0 - 397 °C |
Decomposition Temperature | 431 - 570 °C |
UL RTI, Electrical | 50.0 - 160 °C |
UL RTI, Mechanical with Impact | 50.0 - 130 °C |
UL RTI, Mechanical without Impact | 50.0 - 160 °C |
Flammability, UL94 | V-0 - 5VA |
Flame Spread Index | 0.000 - 5.00 |
Oxygen Index | 30.0 - 53.0 % |
Glow Wire Test | 850 - 960 °C |
|
Optical Properties | Original Value | Comments |
---|
Haze | 0.100 - 2.00 % |
Transmission, Visible | 58.0 - 91.6 % |
|
Processing Properties | Original Value | Comments |
---|
Processing Temperature | 371 - 420 °C |
Nozzle Temperature | 375 - 405 °C |
Melt Temperature | 370 - 416 °C |
Mold Temperature | 135 - 232 °C |
Drying Temperature | 150 - 204 °C |
Moisture Content | 0.0100 % |
Dew Point | -40.0 °C |
Injection Pressure | 138 - 193 MPa |
Vent Depth | 0.00250 - 0.00760 cm |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.