MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP NORYL® PX2926 Polyphenylene Ether + Polystyrene, Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: 5VA rated at 2.5 in black and 3.0 in gray.

  • Features: High Strength
  • Forms: Pellets
  • Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 107 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 4.0 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 141 MPa(102 mm Span) 3mm/min; ASTM D790
Flexural Modulus 8.47 GPa(102 mm Span) 3mm/min; ASTM D790
Izod Impact, Notched 0.587 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 119 sec(Tungsten Electrode, 3.18 mm) (PLC = 6); ASTM D495
Comparative Tracking Index 100 - 174 V
@Thickness 3.18 mm
PLC = 4; UL 746
Hot Wire Ignition, HWI >= 120 sec
@Thickness 3.18 mm
PLC = 0; UL 746
High Amp Arc Ignition, HAI <= 15 arcs
@Thickness 3.18 mm
PLC = 4; UL 746
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
@Thickness 3.18 mm
PLC = 4; UL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
UL RTI, Electrical 50.0 °CUL 746
UL RTI, Mechanical with Impact 50.0 °CUL 746
UL RTI, Mechanical without Impact 50.0 °CUL 746
Flammability, UL94 V-1
@Thickness 1.47 mm
 V-0
@Thickness 3.00 mm
 5VA
@Thickness 2.57 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 304 °C
Middle Barrel Temperature 271 - 310 °C
Front Barrel Temperature 282 - 316 °C
Nozzle Temperature 293 - 316 °C
Melt Temperature 293 - 316 °C
Mold Temperature 76.7 - 104 °C
Drying Temperature 104 - 110 °C
Dry Time 3 - 8 hour
Moisture Content 0.020 %Suggested
Back Pressure 0.345 - 0.689 MPa
Shot Size 30 - 70 %Suggested
Screw Speed 20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® LN30 m-Polyphenylene Ether (m-PPE)
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy
Mitsubishi Iupiace® LN40 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN30 m-Polyphenylene Ether (m-PPE)

PZLNP1273 / 51355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.