MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Iupiace® LN30 m-Polyphenylene Ether (m-PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Flame retardant V-0 grade. Iupiace is a polymer alloy made by modifying PPE with high impact polystyrene (HIPS), nylon-6 or nylon-66. Usability in a wide range of temperatures (-40 to 160). Higher rigidity, impact strength and fatigue resistance. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Flame retardance and excellent self-extinguishing properties. Low density. Low shrinkage rate, ensuring quality precision parts. Good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Water Absorption 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
Immersion
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 300 °C
18 g/10 min
@Load 4.76 lb,
Temperature 572 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psiISO-527-1,2
Elongation at Break 25 %25 %ISO 527-1,2
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 2.40 GPa348 ksiISO 178
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179-1,2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohm2.00e+15 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 55.0 µm/m-°C30.6 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 58.0 µm/m-°C32.2 µin/in-°FISO 11359-2
Maximum Service Temperature, Air 160 °C320 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1,2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94  V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® AN70 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AN80 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN20 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN10 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN30 m-Polyphenylene Ether (m-PPE)

PMITSU9123 / 191796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.