MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Axiall SP-6235 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionally high impact strength, especially at low temperatures. SP-6235 also carries an elevated UL Relative Thermal Index rating.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmASTM D-955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5400 psiASTM D-638
Tensile Modulus 320000 psiASTM D-638
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 3.17 mm,
Temperature -40.0 °C
ASTM D-256
 3.10 ft-lb/in
@Thickness 3.17 mm,
Temperature -20.0 °C
ASTM D-256
 13.5 ft-lb/in
@Thickness 3.17 mm,
Temperature 0.000 °C
ASTM D-256
 20.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 154.4 °Funannealed; ASTM D-648
 167 °Fannealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 141.8 °Funannealed; ASTM D-648
 156.2 °Fannealed; ASTM D-648
Vicat Softening Point 191 °Fannealed; ASTM D-1525A
UL RTI, Electrical 95.0 °CUL-746B
UL RTI, Mechanical with Impact 85.0 °CUL-746B
UL RTI, Mechanical without Impact 95.0 °CUL-746B
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 2.03 mm
 V-0
@Thickness 3.00 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa JH830 Flame Retardant PC
IPB Bicell® Cellular Polypropylene Sheet
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer
Hyosung Topilene B201Y PP
Geon® Performance Solutions Vinyl Packaging PK8 WHITE 1081 Polyvinyl Chloride, Rigid

PGGUL478 / 41754

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.