MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

IPB Bicell® Cellular Polypropylene Sheet
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Extruded, layered PP sheet, with a cellular core layer. Attributes include:
  • Enhanced strength/thickness ratio
  • Omni-directional flexural stresistance
  • High compression strength
  • Wide variety of finishes
  • Recyclable
  • Food approved
  • Resistant to water and humidity
  • Good resistance to grease, oils and most chemicals
  • Sterilizable
Uses include packaging, including food, and displays.

Property data reported here is based on PP raw material - not the formed sheet structure.

Information provided by IPB Plastic Sheet Extrusion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.907 g/cc0.0328 lb/in³ISO 1183
Water Absorption 0.02 %0.02 %ISO 62
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 2.25
@Frequency 1e+6 Hz
2.25
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 70.0 kV/mm1780 kV/inASTM D149
Dissipation Factor <= 0.000500
@Frequency 1e+6 Hz
<= 0.000500
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C100 µin/in-°FASTM D696
Specific Heat Capacity 1.68 J/g-°C0.402 BTU/lb-°FDSC
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °FISO 75
Vicat Softening Point  78.0 °C
@Load 5.10 kg
172 °F
@Load 11.2 lb
ISO 306
 148 °C
@Load 1.02 kg
298 °F
@Load 2.25 lb
ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hifax CB 1160 G1 G41440 Polypropylene
Evonik Cyrolon® AR Polycarbonate Sheet
Total PPH 3061 Polypropylene, Homopolymer
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer
ExxonMobil PP7011L1 Polypropylene Impact Copolymer

PIPBV95 / 142929

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.