System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive
Categories:
Polymer
;
Adhesive
Material Notes:
Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Solids Content
17.4 %
aerosol
29 %
bulk
Volatile Organic Compounds (VOC) Content
576
g/l
Mechanical Properties
Original Value
Comments
Shear Strength
467
psi
@Temperature 121 °C
Overlap, 1/8" Alum/Alum
607
psi
@Temperature 93.0 °C
Overlap, 1/8" Alum/Alum
897
psi
@Temperature 66.0 °C
Overlap, 1/8" Alum/Alum
1306
psi
@Temperature 24.0 °C
Overlap, 1/8" Alum/Alum
3409
psi
@Temperature -34.0 °C
Overlap, 1/8" Alum/Alum
Peel Strength
1.20
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Treated plywood, 1 surface Bond
3.00
pli
After 2 week exposure to 71°C, Vinyl-Altro to Treated plywood, 1 surface Bond
6.70
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Composite, 1 surface Bond
6.70
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Stainless Steel, 1 surface Bond
7.00
pli
After 2 week exposure to 71°C, Vinyl-Altro to Composite, 1 surface Bond
7.00
pli
After 2 week exposure to 71°C, Vinyl-Altro to Stainless Steel, 1 surface Bond
8.30
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Treated plywood, 1 surface Bond
8.70
pli
After 2 week exposure to 71°C, Vinyl-Altro to Stainless Steel, 2 surface Bond
8.70
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Composite, 1 surface Bond
8.70
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Stainless Steel, 1 surface Bond
11.3
pli
After 2 week exposure to 71°C, Vinyl-Altro to Treated plywood, 2 surface Bond
11.3
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Stainless Steel, 2 surface Bond
12.3
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Treated plywood, 2 surface Bond
12.3
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Stainless Steel, 2 surface Bond
13.3
pli
After 2 week exposure to 71°C, Vinyl-Altro to Composite, 2 surface Bond
15.7
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Treated plywood, 2 surface Bond
18.3
pli
After 2 week exposure to 71°C, Vinyl-Gerfor NT to Composite, 2 surface Bond
20.3
pli
After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Composite, 2 surface Bond
7.00
pli
@Temperature 66.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
13.5
pli
@Temperature 24.0 °C,
Time 432000 sec
180°, Canvas/Steel
16.5
pli
@Temperature 24.0 °C,
Time 86400 sec
180°, Canvas/Steel
17.5
pli
@Temperature -34.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
27.5
pli
@Temperature 24.0 °C,
Time 605000 sec
180°, Canvas/Steel
31.0
pli
@Temperature 24.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
Descriptive Properties
Appearance
Light tan
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Innospec FLEXAREN® 18001 EVA-Copolymer
H.C. Starck HPM 1801 Tungsten High Density Composite
DuPont Mobility and Materials Kalrez® 9500 Fluoroelastomer
Cookson Group STAYSTIK® 682 Aluminum Nitride Filled Thermally Enhanced Film
Arlon Electronic Materials 33N Polyimide Laminate and Prepreg
PMM34122 / 168869
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.