MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Transformer Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is also suited for use in circuit breakers, switches and any other oil-immersed electrical equipment. It meets the requirements of ANSI/ASTM D3487 Type II for inhibited oils. This specification provides uniform functional characteristics for petroleum electrical-insulating oil and is recognized by the Institute of Electrical and Electronic Engineers (IEEE) and other professional societies that deal with insulating materials. It also meets Westinghouse Specification PDS 55822AG and Federal Specification VV-L-530A.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.28 lb/gal
@Temperature 15.6 °C
Moisture Absorption <= 0.00200 %
Viscosity Measurement 72Viscosity Index
Saybolt Viscosity at 100°F 56 SUS
Saybolt Viscosity at 210°F 34 SUS
Kinematic Viscosity at 40°C (104°F) 9.0 cSt
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
ASTM Color 0.50
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 32000 VVDE Electrodes at 60 hertz (0.04 inch gap)
 47000 VDisc Electrodes at 60 hertz
 60000 VVDE Electrodes at 60 hertz (0.08 inch gap)
 
Thermal PropertiesOriginal ValueComments
Pour Point -67.0 °F
Rotating Bomb Oxidation Test (RBOT) 300 minASTM D2272
Flash Point 315 °F
 
Descriptive Properties
Acid/Sludge Test0.0172 Hours
 0.03162 Hours
Aniline Point172°F
Approved Antioxidant Content0.26 wt.%
Corrosive SulfurNoncorrosive
Gassing Tendency-14.5 cc/min 80°C
Interfacial Tension 46 dynes/cm25°C
Neutralization No.Max 0.01
Polychlorinated Biphenyls (PCBs)Nil
Power Factor0.003 %60 hertz, 25°C
 0.087 %60 hertz, 100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unipetrol PND 33-352-94 Extra Light Fuel Oil
Unipetrol JET A-1 AFQRJOS Issue 18 Jet Kerosene
Unipetrol R2 Heavy Fuel Oil
ChevronTexaco ECO® ISO 46 Hydraulic Oil AW
Phillips 66 MV22 Super Hydraulic Oil

WCON192 / 75229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.