MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unipetrol JET A-1 AFQRJOS Issue 18 Jet Kerosene
Categories: Fluid; Solvent

Material Notes: Jet Kerosene is a mixture of liquid hydrocarbons, with boiling point ranging between 135 and 280°C. It is obtained from crude oil by distillation and by other technological processes. It may contain additives to improve its usage characteristics. Jet kerosene is a flammable liquid class II of fire hazard, with flash point above 38°C.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.775 - 0.840 g/cc0.0280 - 0.0303 lb/in³
Viscosity Measure <= 8.0 cSt
@Temperature -20.0 °C
<= 8.0 cSt
@Temperature -4.00 °F
Evaporation Loss 10 %
@Temperature 205 °C
10 %
@Temperature 401 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature <= -47.0 °C<= -52.6 °F
Flash Point >= 38.0 °C>= 100 °F
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 0.0030 %0.0030 %Mercaptan Sulfur
 0.30 %0.30 %
 
Descriptive Properties
AppearanceVisually pure, light, without mechanical impurities and undissolved water at ambient temperature
Aromatics Content (%), max25
Doctor Testnegative
Resinous Content, mg/100cm³, max7
Sootless Flame Height mm19with 3% naphthalenes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco A Jet Fuel
Phillips 66 Transformer Oil
Unipetrol PND 33-352-94 Extra Light Fuel Oil
Unipetrol R2 Heavy Fuel Oil
ExxonMobil 10W Mobil Hydraulic

PUNIP077 / 82937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.