MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik UNI-CAL® 866-0018 Colorant
Categories: Color; Other Engineering Material; Additive/Filler for Polymer

Material Notes: UNI-CAL® 866 Industrial Machine Colorants are closely controlled machine dispensable dispersions compatible with a variety of non-aqueous industrial and maintenance coatings. The broad compatibility range of these colorants allows the coatings manufacturer to reduce the number of special pigment dispersions normally required for tinting many special chemical coatings. The solvent in these colorants is a low aromatic, fast-evaporating, Rule 66-type solvent.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/cc
Density 15.2 lb/gal
Solids Content 26.7 %vehicle
 60.8 %pigment
Volatile Organic Compounds (VOC) Content 228 g/l
Volatiles 12.5 %
 
Descriptive Properties
ColorantTitanium White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Protective Coating PC-7® Epoxy Paste
Lanxess LEVANYL® Green G-LF Green Pigment
Evonik UNI-CAL® 866-1810 Colorant
Evonik CAL-TINT® 830-2024 Colorant
Evonik AQUASPERSE® II 877-0451 Color Dispersion

PHUMB352 / 81354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.