MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Protective Coating PC-7® Epoxy Paste
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of good strength. PC-7® formulation provides extended working time, giving user ample time to complete larger jobs, reposition work or make changes. High wet grab or tack of PC-7® makes overhead and sidewall work easy without drip or sag. PC-7® demonstrates excellent chemical resistance to mild acids, caustics, detergents, gasoline, fuel oil, salt, and fresh water. PC-7® will not bond to wax paper, TEFLON®, polyethylene, and some soft plastics.

Data provided by the manufacturer.

Key Words: PC Epoxy
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
Water Absorption 0.44 %0.44 %ASTM C413
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 76761 Week Cure; ASTM D2240
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Yield Strength 20.0 MPa2900 psiASTM D580
Compressive Yield Strength 29.0 MPa4210 psiASTM D695
Adhesive Bond Strength 15.0 MPa2180 psiTensile Shear Strength; ASTM D1002
Gardner Impact 18.0 J13.3 ft-lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °F
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C120 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess LEVANYL® Green G-LF Green Pigment
Evonik UNI-CAL® 866-1810 Colorant
Evonik UNI-CAL® 866-0018 Colorant
Evonik COLORTREND® PLUS™ 802-2009 Universal Machine Colorant
Evonik COLORTREND® 888-9944 Universal Machine Colorant

PEPXP0 / 36418

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.