MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Supplied as killed, semikilled, rimmed, and capped steel. Good weldability, relatively soft and strengthen with cold work during forming or drawing. Widely used in cold forming operations such as heading, upsetting, and extrusion. Used in the as-rolled condition as bar, shapes, sheet, and strip.

Key Words: UNS G10160, ASTM A29, ASTM A108, ASTM A510, ASTM A513, ASTM A545, carbon steels, ASTM A548, ASTM A549, ASTM A576, ASTM A659, MIL SPEC MIL-S-866, SAE J403, SAE J412, SAE J414, DIN 1.0419, DIN 1.1142, DIN GS-Ck16, DIN RSt44.2, DIN 17115 1.0467, DIN 17115 1.0468, DIN 17115 15Mn3, DIN 17115 15Mn3Al, BS 3059 440, BS 3606 440, BS 970 080A15, BS 970 080M15, BS 970 170H15, BS 970 173H16, EN32, AISI1016
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 111
Hardness, Knoop 129Converted from Brinell
Hardness, Rockwell B 64Converted from Brinell
Hardness, Vickers 115Converted from Brinell
Tensile Strength, Ultimate 380 MPa
Tensile Strength, Yield 205 MPa
Elongation at Break 25 %in 50 mm
Reduction of Area 50 %
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000160 ohm-cm
@Temperature 0.000 °C
annealed condition
 0.0000220 ohm-cm
@Temperature 100 °C
annealed condition
 0.0000290 ohm-cm
@Temperature 200 °C
annealed condition
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 °C
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
Typical for steel
Specific Heat Capacity 0.481 J/g-°C
@Temperature >=100 °C
annealed
 0.515 J/g-°C
@Temperature 150 - 200 °C
 0.595 J/g-°C
@Temperature 350 - 400 °C
Thermal Conductivity 51.9 W/m-Kestimated based on similar materials
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.12 - 0.18 %
Iron, Fe 99.13 - 99.58 %As remainder
Manganese, Mn 0.60 - 0.90 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1015 Steel, as rolled

M1016B / 6806

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.