MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of both raw materials, for example the good processability and soft haptic of a TPE-S with the excellent mechanical properties and abrasion resistance of a TPE-U. OnFlex™-U 5300 compounds are formulated to deliver very good scratch resistance, a wide hardness range and good chemical resistance.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ISO 868
Tensile Strength at Break 33.0 MPaISO 37
Tensile Stress at Strain 4.60 MPa
@Strain 100 %
ISO 37
 10.4 MPa
@Strain 300 %
ISO 37
Elongation at Break 540 %ISO 37
Abrasion 55[mm³]; ISO 47469
Compression Set 31 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 69 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 170 - 210 °C
Mold Temperature 30.0 - 60.0 °C
Drying Temperature 100 °C
Dry Time 2.00 hour
 
Descriptive Properties
FeaturesGood Abrasion Resistance
 Oil Resistant
 Scratch Resistant
FormsPellets
Generic MaterialTPE
Generic Material TypeThermoplastic Polyurethane Elastomer (TPU)
Generic NameThermoplastic Elastomer (TPE)
Injection RateSlow
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Consumer Applications
 General Purpose
 Industrial Applications
 Power/Other Tools

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ U 5470A-E0083 Thermoplastic Elastomer (TPE)
Avient OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
Avient OnFlex™ U 5370A-S0015 Thermoplastic Elastomer (TPE)
Avient OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)
Avient OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)

PH0POL1167 / 145736

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.